Typical characteristics | Method | Gazpromneft Reductor CLP 100 |
---|---|---|
Kinematic Viscosity - at 100 °С, mm²/s |
|
100 |
Flash Point (COC), °С | ASTM D 92 | 240 |
Pour Point, °С | ГОСТ 20287 | - 20 |
Total Acid Number, mg KOH/g | ГОСТ 11362 | 0.7 |
Density - at 20 °С, g/cm³ |
ASTM D 4052 |
0.888 |
Viscosity Index | ASTM D 2270 | 92 |
Tribological characteristics, Four-Ball Method - Load-wear index, N - Wear Scar Diameter, mm |
ГОСТ 9490 ГОСТ 9490 |
464 0.26 |
Corrosion of the copper - 24 hours at 120 °C |
ASTM D 130 |
1в |